Analysis Of The Effect Of Welding Current Variations In The SMAW Process On The Stress-Strain Characteristics And Hardness Of Ductile Cast Iron
DOI:
https://doi.org/10.26740/jtm.v15n04.p89-94Abstract
Nodular cast iron is widely used in bearing housing components due to its wear resistance, high toughness, and good machinability. However, the welding process on nodular cast iron often degrades its mechanical properties due to high thermal cycling. This experimental study analyzes the effect of varying SMAW welding currents of 80A, 90A, and 100A using a 2.6-mm-diameter ENiFe-CI electrode on the stress-strain characteristics and hardness of welded joints in 6-mm-thick FCD 500 nodular cast iron, with a single V-butt joint, a 60° bevel angle, and the 1G position. Tensile testing was conducted in accordance with ASTM E8/E8M, and Vickers hardness testing was performed in accordance with ASTM E92 on the WM, HAZ, and BM zones. The test results showed a consistent decrease in tensile strength from 512.61 MPa at 80A to 480.82 MPa at 90A and 402.34 MPa at 100A, a 21.5% decrease from 80A to 100A, followed by a 61.82% decrease in tensile strain (from 3.30% to 1.26%), indicating that the material became increasingly brittle. This decrease is believed to be related to the coarsening of the dendritic structure in the WM and the degradation of the nodular graphite morphology accompanied by matrix softening in the HAZ due to increased heat input. The hardness in the WM and HAZ also decreased by 7.07% and 6.81%, respectively, from 80A to 100A, while the BM remained relatively stable across welding currents (a difference of 0.2 HVN or 0.07%) because it was far from the heat source, but remained approximately 9.38% lower than that of the raw material. These results are descriptive of three replicates; the 80A current condition yielded the best results among the tested conditions.
Downloads
Downloads
Published
Issue
Section
Abstract views: 15
,
PDF Downloads: 11